Graphene Oxide Washing

Cite This in Your Publication

Graphene Oxide Washing - InstaNANO. https://instanano.com/all/nanomaterial-synthesis/carbon/graphene-oxide-2/ (accessed March 28th, 2024).

Graphene Oxide washing is very crucial task which can be done by washing it multiple times with HCL and Deionized water.

  1. CHECK LIST
    Hydrochloric Acid (HCL), Graphene Oxide (GO), Deionized Water, Centrifuge Tubes and Centrifuge Machine.

  2. STEP 1.
    Add 100ml Hydrochloric Acid in 900ml deionized water and wash Graphene Oxide with it several times for 15-20 minutes each at 5000rpm.

  3. STEP 2.
    Wash again with deionized water 5-6 times for 30 minutes each at 6000rpm.

  4. RESULTS
    After washing from second step Graphene Oxide volume would be increased with decrease in density and it looks like potter’s clay.

  5. Factors Affecting Synthesis
    Concentration of HCL: Hydrochloric Acid (HCL) is used in the washing process of Graphene Oxide (GO) because HCL can remove/dissolve any metal impurity during the synthesis of GO from Hummers method. By using concentrated HCL partial reduction of GO may be possible.
    Centrifuge Time and Speed: Centrifuge time and speed (rpm) decide the amount of GO settle down in the centrifuge tube. At higher speed and more time washing, even smaller size GO can settle down in the centrifuge tube.
    Number of Washing: How many times you wash is very important in this washing process. More times you wash the GO, leads to good quality GO with less impurities.

  6. NOTE: All the experiments should be done under the guidance of lab Incharge; and proper lab safety instructions.